研討會論文

  • Yi-En Ke, Yung-I Chen*, Mechanical properties and bonding characteristics of magnetron sputtered ZrNx films, ISPlasma2020, Nagoya, 2020. (MOST 106-2221-E-019-022-MY3)
  • Yi-En Ke, Ting-En Lu, Rong-Tan Huang, Yung-I Chen*, Preparation of ZrO2 top coat by APPJ on laminated RuAl/RuAlZr coatings, ISPlasma2020, Nagoya, 2020. (MOST 106-2221-E-019-022-MY3)
  • Yung-I Chen*, Yi-En Ke, Ming-Ching Sung, Li-Chun Chang, Rapid thermal annealing of Cr-Si-N, Ta-Si-N, and Zr-Si-N coatings in glass molding atmospheres, TACT2019, Taipei, 2019. (MOST 105-2221-E-019-007-MY3)
  • Yi-En Ke, Yung-I Chen*, Mechanical properties, bonding characteristics, and thermal stability of magnetron sputtered HfNx films, TACT2019, Taipei, 2019. (MOST 107-2813-C-019-019-E, 105-2221-E-019-007-MY3)
  • Yi-En Ke, Yung-I Chen*, Effects of Nitrogen Flow on the Mechanical Properties and Bonding Characteristics of Hf-N Films, ISSP2019, Kanazawa, 2019. (MOST 107-2813-C-019-019-E, 105-2221-E-019-007-MY3)
  • Yung-I Chen*, Hsien-Hao Lo, Thermal stability of multilayered Ru-Si-Zr coatings on Inconel 617, ISSP2019, Kanazawa, 2019. (MOST 106-2221-E-019-022-MY3)
  • Yu-Heng Liu, Li-Chun Chang, Bo-Wei Liu, Yung-I Chen*, Characterization of Cosputtered W-Si-N Coatings, ICMCTF2019, San Diego, 2019. (MOST 105-2221-E-019-007-MY3)
  • Yung-I Chen*, Yu-Zhe Zheng, Li-Chun Chang, Effect of bias voltage on mechanical properties of Zr-Si-N films fabricated through HiPIMS/RFMS cosputtering, ICMCTF2019, San Diego, 2019. (MOST 105-2221-E-019-007-MY3)
  • Yu-Heng Liu, Li-Chun Chang, Yung-I Chen*, Yu-Heng Liu, Li-Chun Chang,Yung-I Chen, Mechanical properties and microstructure of sputtered V-Si-N coatings, ISPlasma2019, Nagoya, 2019. (MOST 105-2221-E-019-007-MY3)
  • Yu-Heng Liu, Yung-I Chen*, Mechanical properties of sputtered Cr-Si-N coatings, ISPlasma2019, Nagoya, 2019. (MOST 105-2221-E-019-007-MY3)
  • Li-Chun Chang, Yu-Zhe Zheng, Yung-I Chen*, Mechanical Properties of Zr-Si-N Thin Films Fabricated through HIPIMS/RFMS Cosputtering, ThinFilms2018, Shenzhen, 2018. (MOST 105-2221-E-019-007-MY3)
  • Yung-I Chen*, Jia-Wei Jhang, Oxidation resistance of Ru-Al/Ru-Al-Zr multilayer coatings on Inconel 617, ThinFilms2018, Shenzhen, 2018. (MOST 106-2221-E-019-022-MY3)
  • Yung-I Chen*, Jia-Wei Jhang, Oxidation behavior of RuAlZr multilayer coatings, ISPlasma2018, Nagoya, 2018. (MOST 106-2221-E-019-022-MY3)
  • Yung-I Chen*, Zhi-Ting Zheng, Jia-Wei Jhang, Thermal stability of Ru-Al multilayer coatings on Inconel 617, TACT2017, Hualien, 2017. (MOST 106-2221-E-019-022-MY3)
  • Yung-I Chen*, Nai-Yuan Lin, Li-Chun Chang, Oxidation behavior of Ti-Si-N coatings with cyclical gradient concentration, TACT2017, Hualien, 2017. (MOST 105-2221-E-019-007-MY3)
  • Yung-I Chen*, Yu-Xiang Gao, Li-Chun Chang, Yi-En Ke, Mechanical properties and bonding characteristics of Nb-Si-N coatings with cyclical gradient concentration, TACT2017, Hualien, 2017. (MOST 105-2221-E-019-007-MY3)
  • Yung-I Chen*, Zhi-Ting Zheng, Nai-Yuan Lin, Oxidation behaviors of laminated Al-Hf and Al-Ta coatings, ISSP2017, Kanazawa, 2017. (MOST 102-2221-E-019-007-MY3)
  • Yung-I Chen*, Bo-Wei Liu, Li-Chun Chang, Oxidation behavior of Hf-Si-N coatings with cyclic gradient concentration, ICASS2017, Dalian, 2017. (MOST 105-2221-E-019-007-MY3)
  • Yung-I Chen*, Shan-Chun Chang, Li-Chun Chang, Yu-Zhe Zheng, Jyh-Wei Lee, X-ray photoelectron spectroscopy study of Zr-Si-N coatings, ICASS2017, Dalian, 2017. (MOST 105-2221-E-019-007-MY3)
  • Yung-I Chen*, Yu-Xiang Gao, Li-Chun Chang, Oxidation Behavior of Nb-Si-N Coatings, ICMCTF2017, San Diego, 2017. (MOST 105-2221-E-019-007-MY3)
  • Yung-I Chen*, Yu-Xiang Gao, Li-Chun Chang, Oxidation Resistance of Ta-Si-N Coatings, ICMCTF2017, San Diego, 2017. (MOST 105-2221-E-019-007-MY3)
  • Y.I. Chen*, S.C. Chang, L.C. Chang, Mechanical and tribological properties of Zr-Si-N coatings, ThinFilms2016, Singapore, 2016.
  • Y.I. Chen*, Z.T. Zheng, Y.R. Huang, Oxidation behavior of Ru-Al multilayer coatings, ThinFilms2016, Singapore, 2016. (MOST 102-2221-E-019-007-MY3)
  • L.C. Chang*, Y.Z. Zheng, Y.X. Gao, Y.I. Chen, Tribological behavior of sputtered Cr-W-N coatings, ThinFilms2016, Singapore, 2016. (MOST 102-2221-E-019-007-MY3)
  • Y.I. Chen*, S.C. Chang, L.C. Chang, Characterization of Zr-Si-N coatings prepared using direct current magnetron co-sputtering", TACT2015, Tainan, 2015. (MOST 102-2221-E-019-007-MY3)
  • Y.I. Chen*, J.H. Lin, Y.R. Cheng, C.C. Chou, Oxidation resistance and mechanical properties of TaAlN coatings", TACT2015, Tainan, 2015. (MOST 102-2221-E-019-007-MY3)
  • Y.I. Chen*, T.S. Lu, Mechanical properties of internally oxidized Ru-Zr coatings, TACT2015, Tainan, 2015. (MOST 102-2221-E-019-007-MY3)
  • Y.I. Chen*, Thermal stability and chemical inertness of nitride coatings in glass molding, The 1st international Workshop on Advanced Plasma Technology and Application, New Taipei, 2015. (MOST 102-2221-E-019-007-MY3)
  • L.C. Chang*, Y.I. Chen, C.Y. Chang, H.L. Kao, The mechanical properties and oxidation resistance of ZrxN thin films by high power impulse magnetron sputtering, ISSP2015, Kyoto, 2015.
  • Y.I. Chen*, Y.R. Cheng, J.W. Lee, Thermal stability and chemical inertness of Cr-W-N coatings in glass molding, ISSP2015, Kyoto, 2015. (MOST 102-2221-E-019-007-MY3).
  • Y.I. Chen*, Y.R. Huang, L.C. Chang, Internal oxidation behavior of laminated Hf-Ru coatings, ISSP2015, Kyoto, 2015. (MOST 102-2221-E-019-007-MY3)
  • Y.I. Chen*, T.S. Lu, Mechanical Properties of Internally Oxidized Ru-Zr Coatings, ICMCTF2015, San Diego, 2015. (MOST 102-2221-E-019-007-MY3)
  • Y.I. Chen*, Y.R. Huang, Oxidation behavior and mechanical properties of laminated Hf-Ta coatings, VASSCAA-7, Hsinchu, 2014. (MOST 102-2221-E-019-007-MY3)
  • L.C. Chang*, Y.I. Chen, C.Y. Chang, H.H. Wang, Effects of the Zr content on the mechanical properties and oxidation resistance of reactively sputtered Ta1-xZrxN thin films, ThinFilms2014, Chongqing, 2014. (MOST 102-2221-E-019-007-MY3)
  • Y.I. Chen*, K.C. Lin, Y.R. Huang, Oxidation behavior and mechanical properties of laminated Ta-Ti and Ta-Hf coatings, ThinFilms2014, Chongqing, 2014. (MOST 102-2221-E-019-007-MY3)
  • Y.I. Chen*, Y.R. Cheng, L.C. Chang, Y.H. Chen, T.S. Lu, The chemical inertness of TaSiN coatings in glass molding processes, ThinFilms2014, Chongqing, 2014. (MOST 102-2622-E-019-003-CC3)
  • Y.I. Chen*, Y.R. Cheng, L.C. Chang, Y.H. Chen, Chemical Inertness of Ta-Si-N Coatings with Lanthanum Borosilicate Glasses, ICMCTF2014, San Diego, 2014. (MOST 102-2622-E-019-003-CC3)
  • Y.I. Chen*, H.H. Wang, Oxidation Resistance and Mechanical Properties of CrTaSiN Coatings, ICMCTF2014, San Diego, 2014. (MOST 102-2622-E-019-003-CC3)
  • Y.I. Chen*, Internal oxidation of nanolaminated coatings, ICMCTF2014, San Diego, 2014. (MOST 102-2221-E-019-007-MY3)
  • Y.I. Chen*, K.Y. Lin, H.H. Wang, K.C. Lin, Thermal stability of TaN, CrTaN, TaSiN, and CrTaSiN hard coatings in oxygen containing atmospheres, TACT2013, Taipei, 2013. (NSC 101-2221-E-019-034)
  • S.C. Liu, Y.I. Chen*, J.J. Shyu, H.Y. Tsai, K.Y. Lin, Y.H. Chen, K.C. Lin, Chemical inertness of Ir-Re and Ta-Ru coatings with B2O3-ZnO-La2O3 based glass in glass molding processes, TACT2013, Taipei, 2013. (NSC 101-2622-E-019-004-CC3)
  • Y.I. Chen*, H.N. Chu, L.C. Chang, J.W. Lee, Internal oxidation and mechanical properties of Ru based alloy coatings, ISSP2013, Kyoto, 2013. (NSC 101-2221-E-019-034)
  • S.C. Liu, Y.I. Chen*, H.Y. Tsai, K.C. Lin, Y.H. Chen, Thermal stability of Ir-Re coatings annealed in oxygen containing atmospheres, ICMCTF2013, San Diego, 2013. (NSC 101-2622-E-019-004-CC3)
  • Y.I. Chen*, H.N. Chu, Internal Oxidation of nanolaminated Nb-Ru Coatings, ICMCTF2013 , San Diego, 2013. (NSC 101-2221-E-019-034)
  • Y.I. Chen*, K.Y. Lin, Oxidation resistance and mechanical properties of TaSiN coatings, ICMCTF2013, San Diego, 2013. (NSC 101-2622-E-019-004-CC3)
  • Y.I. Chen*, K.Y. Lin, C.C. Chou, CrTaN hard coatings prepared by biased DC sputter deposition, ThinFilms2012, Singapore, 2012.
  • Y.I. Chen*, S.M. Chen, L.C. Chang, XPS and TEM studies on internally oxidized Nb-Ru coatings, ThinFilms2012, Singapore, 2012.
  • Y.I. Chen*, S.M. Chen, Annealing effects on microstructure and mechanical properties of nanolaminated Ta-Zr coatings, ICMCTF2012, San Diego, 2012.
  • Y.I. Chen*, S.M. Chen, Oxidation Study of Ta-Zr Coatings, TACT2011, Kenting, 2011. (NSC-99-2221-E-019-009)
  • L.C. Chang*, Y.I. Chen, Oxidation Study of Nanocrystalline Cr-Ta Hard Coatings, TACT2011, Kenting, 2011. (NSC 99-2221-E-131-039)
  • Y.I. Chen*, S.M. Chen, Laminated Structure in the internally oxidized Ru-Ta coatings, IUMRS-ICA 2011, Taipei, 2011. (NSC-99-2221-E-019-009)
  • Y.I. Chen*, S.M. Chen, Laminated Structure in the internally oxidized Ta-Ru coatings, ICMCTF2011, San Diego, 2011. (NSC-99-2221-E-019-009)
  • Y.I. Chen*, Y.T. Lin, Preparation and annealing study of CrTaN coatings on WC-Co substrates, ICMCTF2011, San Diego. 2011. (NSC-99-2221-E-019-009)
  • Y.I. Chen*, B.N. Tsai, Initial Stage of Internal Oxidation of Ta-Ru and Mo-Ru Coatings, ThinFilms2010, Harbin, 2010. (NSC-98-2221-E-019-009)
  • Y.I. Chen*, B.L. Lin, Y.C. Kuo, TaNx Diffusion Barrier on Cobalt Cemented Tungsten Carbide, ICMCTF2010, San Diego, 2010. (NSC-98-2221-E-019-009)
  • B.N. Tsai, Y.I. Chen*, Oxidation Study of Ta-Ru Hard Coatings, ICMCTF2010, San Diego, 2010. (NSC-98-2221-E-019-009)
  • Y.I. Chen*, B.N. Tsai, Microstructure and Mechanical Properties of Ta-Ru Coatings on Tungsten Carbide, TACT2009, Taipei, 2009. (NSC-98-2221-E-019-009)
  • Y.I. Chen*, L.C. Chang, R.T. Huang, B.N. Tsai, Effect of Annealing Atmosphere on the Oxidation Behavior of Mo-Ru Coatings, TACT2009, Taipei, 2009. (NSC-97-2218-E-019-002)
  • Y.I. Chen*, Oxidation Study of Mo-Ru Hard Coatings, ICMCTF2009, San Diego, 2009. (NSC-97-2218-E-019-002)
  • Y.I. Chen*, L.C. Chang, B.N. Tsai, Interlayer Effect on the Detaching Mechanism for Mo-Ru Hard Coatings, ICMCTF 2009, San Diego, 2009. (NSC-97-2218-E-019-002)
  • Y.I. Chen*, L.C. Chang, J.W. Lee, Y.C. Kuo, C.J. Wang, Annealing Study of Mo-Ru Hard Coatings on Tungsten Carbide, ICMCTF 2008, San Diego, 2008.
  • L.C. Chang*, Y.I. Chen, J.W. Lee, H.Y. Lin, Y.C. Kuo, C.J.Wang, Detaching mechanism for Mo-Ru hard coating on tungsten carbide, ICMCTF 2007, San Diego, 2007.
  • Y.I. Chen, J.J. Li, M.S. Tsai, C.H. Yeh, M.H. Hon, Powder Preparation and Sintering of Grain Growth Controlled Cr2O3-ZrO2 Composites, 96th Annual Meeting of the American Ceramic Society, Cincinnati, 1994.
  • J.G.. Duh, Y.I. Chen, Interlayer Modified TiN Coating on Carbon Steels, Proceeding of the International Ceramic Conference Australia 1992, Melburne, 1992.
  • 羅憲豪、陳永逸、陳君彥,磁控濺鍍Ru-Al-Ti鍍層之氧化行為,2019材料年會,台南。(MOST 106-2221-E-019-022-MY3)
  • 柯懿恩、陳永逸,大氣下多層鍍層Al-Ta之氧化行為,2019材料年會,台南。(MOST 106-2221-E-019-022-MY3)
  • 羅憲豪、陳永逸,磁控濺鍍Si-Ru-Zr鍍層之氧化行為,2018材料年會,台中。(MOST 106-2221-E-019-022-MY3)
  • 李錦松、劉宇恆、陳永逸,反應式磁控濺鍍 Mo-Si -N鍍層,2018材料年會,台中。(MOST 105-2221-E-019-007-MY3)
  • 劉柏緯、劉宇恆、陳永逸,氮氣流率及基板轉速對磁控濺鍍WxSiyN(100-x-y)鍍層之效應,2018材料年會,台中。(MOST 105-2221-E-019-007-MY3)
  • 柯懿恩、陳永逸,高氮氣氛下反應式磁控濺鍍Hf3N4鍍層之機械性質,TACT2018,新北。(MOST 107-2813-C-019-019-E, 105-2221-E-019-007-MY3)
  • 李錦松、陳永逸,Nb-Ru鍍層在快速退火中之氧化行為,TACT2018,新北。(MOST 106-2221-E-019-022-MY3)
  • 劉柏緯、劉宇恆、陳永逸,矽含量對W-Si-N鍍層之結構與機械性質影響,TACT2018,新北。(MOST 105-2221-E-019-007-MY3)
  • 劉宇恆、陳永逸,磁控濺鍍V-Si-N 薄膜之結構與機械性質,TACT2018,新北。(MOST 105-2221-E-019-007-MY3)
  • 林乃元、陳永逸,熱處理對Ta-Al鍍層結構的影響,2016材料年會,新竹。(MOST 102-2221-E-019-007-MY3)
  • 高裕翔、陳永逸、林乃元,TaSiN鍍層的抗氧化行為,TACT2016,屏東。(MOST 105-2221-E-019-007-MY3)
  • 張善淳、陳永逸,ZrSiN鍍層的XPS研究,TACT2016,屏東。(MOST 105-2221-E-019-007-MY3)
  • 鄭芝婷、陳永逸,層狀Al-Hf鍍層的氧化行為與機械性質,TACT2016,屏東。(MOST 102-2221-E-019-007-MY3)
  • 黃鈺荏、陳永逸、鄭芝婷,層狀Hf-Ru鍍層的內氧化行為,2015材料年會,高雄。(MOST 102-2221-E-019-007-MY3)
  • 鄭玉如、陳永逸*、高裕翔,Cr-W-N鍍膜在玻璃模造的熱穩定性和化學惰性,TVS2015,台北。(MOST 102-2221-E-019-007-MY3)
  • 黃鈺荏、陳永逸*、呂佐紳,Hf-Ta鍍層氧化行為與機械性質,TACT2014,苗栗。(MOST 102-2221-E-019-007-MY3)
  • 林國正、陳永逸*,Ta-Ti 鍍層氧化行為研究,TACT2014,苗栗。(MOST 102-2221-E-019-007-MY3)
  • 王銹惠、陳永逸*,不同氮氣流量比率下製備鉻鉭矽氮化物鍍層的機械性質與抗氧化性,TACT2014,苗栗。(MOST 102-2221-E-019-007-MY3)
  • 林國正、陳永逸*,V-Ru鍍層氧化行為研究,TVS2013,台南。(NSC 101-2221-E-019-034)
  • 朱秀暖、陳永逸*,釕合金鍍層之氧化行為與機械性質。2013年中國材料科學學會年會,桃園 。(NSC 101-2221-E-019-034)
  • 陳永逸*、陳欣敏。內部氧化Nb-Ru鍍層的XPS與TEM研究,2012年中國材料科學學會年會,雲林。(NSC 101-2221-E-019-034)
  • 林昆毅、陳永逸*,TaSiN薄膜機械性質與抗氧化性研究,TACT2012,新北。(NSC 101-2622-E-019-004-CC3)
  • S.M. Chen, Y.I. Chen*, XPS Studies on Oxidation Behaviors of Ta-Ru and Ta-Zr Coatings, TVS2011, Hsinchu. (NSC-99-2221-E-019-009)
  • Y.I. Chen*, K.S. Liao, Z.X. Su, XPS Studies on Oxidation Behavior of Mo-Ru Coatings, TACT2010, ChangHua, (NSC-98-2221-E-019-009)
  • 蔡秉男、陳永逸*,含氧氣氛下Ta-Ru及Mo-Ru薄膜的氧化行為,2010年中國材料科學學會年會,高雄。(NSC-98-2221-E-019-009)
  • 陳永逸*、郭裕竹,含氧氣氛下Cr-Ru硬膜的氧化行為,2010年中國材料科學學會年會,高雄。(NSC-98-2221-E-019-009)
  • 陳永逸*、蔡秉男,含氧氣氛下Mo-Ru硬膜的氧化行為,2009年中國材料科學學會年會,花蓮。 (NSC-97-2218-E-019-002)
  • 陳永逸*、張麗君、李志偉、黎佳霖,Mo-Ru硬膜的氧化行為,2008年中國材料科學學會年會,台北。(NSC-97-2218-E-019-002)
  • 郭裕竹、李志偉*、張麗君、陳永逸、王朝正、黃仁清,以液態原子力顯微鏡即時觀察合金薄膜剝除行為之研究,96年度中華民國防蝕工程學會年會,2007。
  • 楊希文、林育儀、蔡宗儒、陳永逸、林惠娟,添加氧化鉺於氟磷酸鹽玻璃之性質研究, 2005年中國材料科學學會年會。
  • 蔡宗儒、楊希文、林育儀、陳永逸,掺銩磷酸鹽雷射玻璃研究,2005年中國材料科學學會年會。
  • P. Peng, Y.I. Chen, F.B. Wu, Investigation of the mechanical and tribological properties of TiAlN films, 2003年中國材料科學學會年會。
  • 陳永逸、彭珮君、郭孟鑫,無電鍍Ni-Cu-P及Ni-Cu-P-Sb膜層研究,2000年中國材料科學學會年會。.
  • 陳永逸、王俊欽、鄧高生,品質管制技術於模仁材料評估之研究,1999年中國材料科學學會年會,新竹。
  • 陳永逸、韓偉國、王俊欽、龔大焜、鄧高生,非球面CD讀取頭鏡片射出成型與量測技術研究,1998年中國材料科學學會年會,台北。
  • 陳永逸、韓偉國、王俊欽,塑膠鏡片射出成型技術之品質工程研究",1997年中國材料科學學會年會論文集,台南。
  • 陳永逸、鄧高生、王俊欽、魏俊敏、葉柏良,玻璃模造製程技術研究,台灣光電產業技術發展研討會,新竹,1997。
  • 魏俊敏、陳永逸、王俊欽、鄧高生,球狀玻璃預形體製程研究,台灣光電產業技術發展研討會,新竹,1997。
  • 陳永逸、陳錫儀、鄧高生,氧化鉻-氧化鋯複合陶瓷之緻密化與機械性質,1995年中國材料科學學會年會,台中。.
  • Y.I. Chen, J.J. Li, S.H. Shieh, Sintering Kinetics of Chromium Oxide, 1993年中國材料科學學會年會,新竹。.
  • Y.I. Chen, J.J. Li, Inhibition of Grain Growth in Cr2O3 by ZrO2, 1993年中國材料科學學會年會,新竹。
免費建立您的網站! 此網站是在 Webnode 上建立的。今天開始免費建立您的個人網站 立即開始